Dream comes true with technology

Reference suggestion for injection molding of PC/ABS alloy                      

Injection Molding Unit

NH6000D

NHL8000 NHL8800
drying temperature 90-100

80-100

80-100

drying time hrs

4-6

4-6 4-6
maximum humidity ratio %

0.02%

0.02%

0.02%

molding temperature  ℃  240-270 230-270 230-270
mold temperature 40-80 40-80 40-80
back pressure MPa 0.3-0.7 0.3-0.7 0.3-0.7
screw rev rpm 30-80 30-80 30-80
molding ejection volume per time % 30-80 30-80 30-80
injection molding pressure MPa 50-160 50-160 50-160